Whitish appearance, damage usually starting from edges and corners followed by cracking and spalling of concrete is caused by which of the following?
- 1Chloride attack
- 2Acid attack
- 3Sea-water effect
- 4Sulphate attack✓
Correct answer
Sulphate attack