Computer · Highway Materials
When both flakiness and elongation indices are to be determined for a sample of aggregates, what is the correct sequence in which the tests are conducted?
- 1Elongation index test followed by flakiness index test on the non-elongated aggregate fraction
- 2Flakiness index test followed by elongation index test on the non-flaky aggregate fraction✓
- 3Elongation index test followed by flakiness index test on the entire original sample
- 4Flakiness index test followed by elongation index test on the entire original sample
Correct answer
Flakiness index test followed by elongation index test on the non-flaky aggregate fraction
Download Single Question PDF
Save this question and verified answer as a clean study sheet with live clickable link.
Share with Friends & Study Groups
Challenge your peer aspirants on WhatsApp or Telegram to solve this question!
Preparing for Computer?
Practice full-length Computer mock tests with real exam timers, instant score analysis, and all-India ranking.
Want more practice questions on Highway Materials?
Solve complete topic-wise tests with detailed solutions on GkGet.
Related Practice Questions
Recommended practice questions in Computer · Highway Materials