General Studies · Metal Casting Defects
A 'misrun' is a casting defect that primarily occurs due to:
- 1Improper alignment of the mould flasks
- 2Insufficient fluidity of the molten metal✓
- 3Absorption of gases by the liquid metal
- 4Very high pouring temperature of the metal
Correct answer
Insufficient fluidity of the molten metal